Notes
Choosing Shore A Hardness for Seals, Pads and Cases
Two parts can share a drawing and still be different products, because hardness is a separate decision from geometry. Here is what actually changes as you move up and down the Shore A scale.
What Shore A Measures
Shore A measures resistance to indentation on a soft-to-medium scale, read from a durometer pressed into the material. It is not a strength figure and it is not a density figure. A 50 Shore A compound and a 70 Shore A compound can be based on the same polymer; the difference is the filler loading and the cure system.
Silicone for industrial parts normally runs from 30 to 80 Shore A. Below 30 the material becomes difficult to demould and tears easily at thin walls. Above 80 it stops behaving like an elastomer and starts behaving like a hard plastic with poor recovery.
What Changes With Hardness
| Property | Lower hardness (40–50) | Higher hardness (60–70) |
|---|---|---|
| Sealing force at fixed compression | Lower | Higher |
| Compression set resistance | Better recovery | Slower recovery, more set |
| Tear resistance at thin sections | Weaker | Stronger |
| Grip and friction | Higher | Lower |
| Demoulding from a deep cavity | Harder | Easier |
| Deflection under a clip or rib | Softer, more give | Stiffer, holds shape |
Picking a Grade for a Seal
For a static seal in a machined groove, 50 to 60 Shore A is the usual starting point. Softer compounds fill surface irregularities better and seal at lower compression. Harder compounds resist extrusion through a wide gap and hold up better under pressure.
For a dynamic seal, or anything that slides, hardness matters less than compression set. Ask for the compression set figure at your service temperature, not just the hardness number.
Picking a Grade for a Protective Case
A case that has to stay on a device through vibration usually sits at 55 to 65 Shore A: hard enough to hold its shape around the corners, soft enough to absorb a knock. Below 50 the case peels off the corners. Above 70 it transmits impact instead of absorbing it, and the buttons become stiff.
Picking a Grade for a Foot Pad or Gasket
Softer is almost always better here, 40 to 50 Shore A, because the pad has to conform to a surface that is not perfectly flat. The limit is tear resistance: if the pad is thin and slides sideways under load, a harder grade lasts longer.
How to Specify It on a Drawing
Put the hardness on the drawing as a range, not a single number: "50 ± 5 Shore A, ASTM D2240, 1 s reading." A single number invites a debate at inspection that nobody wins. A range with the test method and the reading delay is checkable by both sides.
State the tolerance for every critical dimension at the same time. Hardness and tolerance interact: a soft part in a tight tolerance is more expensive to make than the same part in a harder grade, because soft material moves under the measuring stylus.
FAQ
Can you match the hardness of a sample I send?
Yes. We measure the sample and quote the nearest standard grade. If the sample is outside the usual 30 to 80 Shore A range, we tell you before quoting rather than after.
Does colour affect hardness?
Not directly, but pigment loading can shift it by a few points. When colour and hardness are both critical, we approve the coloured sample rather than the natural one.
---
Send a drawing, a sample or the device model
We reply with a line-item quotation — tooling (NRE) and unit price quoted separately — within one business day.